Fig. 2From: Release characteristics of enoxaparin sodium-loaded polymethylmethacrylate bone cementSME image of ES-PMMA bone cement. a No ES loaded PMMA bone cement. b 40 g PMMA bone cement + 8000 AxaIU ES. c 40 g PMMA bone cement + 16,000 AxaIU ES. d 40 g PMMA bone cement + 24,000 AxaIU ESBack to article page