Skip to main content

Table 6 Significant analysis of in A, B, and C groups

From: Degraded and osteogenic properties of coated magnesium alloy AZ31; an experimental study

Time

Group 1

Group 2

P (tensile strength)

P (flexural strength)

2nd week

    
 

A

B

0.0445

<0.0001

 

A

C

<0.0001

<0.0001

 

B

C

<0.0001

0.0191

4th week

    
 

A

B

0.0104

<0.0001

 

A

C

<0.0001

<0.0001

 

B

C

<0.0001

0.0072

8th week

    
 

A

B

<0.0001

<0.0001

 

A

C

<0.0001

<0.0001

 

B

C

<0.0001

0.0033

12th week

    
 

A

B

<0.0001

<0.0001

 

A

C

<0.0001

<0.0001

 

B

C

<0.0001

<0.0001

  1. Group A means magnesium alloy AZ31 without coating. Group B means magnesium alloy AZ31 with 10-μm coating. Group C means magnesium alloy AZ31 with 20-μm coating