Table 4 Results of tensile strength in A, B, and C groups (MPa, mean ± SEM)

From: Degraded and osteogenic properties of coated magnesium alloy AZ31; an experimental study

Group

2nd week

4th week

8th week

12th week

A

177.08 ± 2.25

161.56 ± 1.54

135.16 ± 1.66

112.92 ± 1.00

B

184.99 ± 0.61

171.93 ± 7.97

154.06 ± 1.85

132.25 ± 7.42

C

206.32 ± 8.50

195.28 ± 6.16

174.38 ± 1.98

153.40 ± 1.68

  1. Group A means magnesium alloy AZ31 without coating. Group B means magnesium alloy AZ31 with 10-μm coating. Group C means magnesium alloy AZ31 with 20-μm coating