From: Effects of reinforcing materials on durability of bone cement: in vitro experimental study
Pressure values (MPa) | p | ||
---|---|---|---|
Min-Max (median) | Mean ± SD | ||
Group 1 (n = 25) | 79.2–81.1 (80.2) | 80.25 ± 0.42 | 0.001 |
Group 2 (n = 25) | 79.5–81.2 (80.7) | 80.46 ± 0.68 | |
Group 3 (n = 25) | 79.0–82.2 (80.5) | 80.73 ± 0.57 | |
Group 4 (n = 25) | 89.1–91.4 (90.5) | 90.41 ± 0.57 |