Fig. 4From: Degraded and osteogenic properties of coated magnesium alloy AZ31; an experimental studyComparison of the bone tissue at 2nd week and 12th week. Group A means magnesium alloy AZ31 without coating. Group B means magnesium alloy AZ31 with 10-μm coating. Group C means magnesium alloy AZ31 with 20-μm coating. Group D means the control groupBack to article page