Fig. 2From: Degraded and osteogenic properties of coated magnesium alloy AZ31; an experimental studyThe changes of magnesium alloy AZ31 from 2nd week to 12th week. Group A means magnesium alloy AZ31 without coating. Group B means magnesium alloy AZ31 with 10-μm coating. Group C means magnesium alloy AZ31 with 20-μm coatingBack to article page